How to understand the solid content of the sealant of the steel pail
Why has the steel bucket had leakage problems many times after we chose a sealant with higher solid content? Many steel pail makers have asked this question. The key issue is that the 'solid content' some sealant manufacturers mentioned is not what we need when producing steel containers.
The solid content of sealant required for steel pail manufacturing is not the solid content by weight, but the solid content by volume. That is to say, if I buy one liter of sealant, there will be 0.7 liters of dry film after curing, and this is the sealant we need. To achieve a high solid content by volume, adding enough natural latex to the sealant is necessary. Natural latex contains very little water, and the volume remains unchanged after drying.
Some suppliers claim that their sealant has a solid content of up to 70%, which means that if you buy one kilogram of sealant, after curing, the dry glue can reach 0.7 kilograms. Is it worth it? These so-called high-value solid contents are just adding more white powder (or other solid powders), which are not worth much. Then add water, and the water will precipitate. The bottom is thick and hard, and the top is thin water. What do they do? Add thickener.
The solid content in terms of weight is calculated by using white powder, and has very little elasticity.
This causes leakage problems in the steel pail.